- The non - equilibrium segregation of boron in matrix grains in fe - cr - b alloys
合金晶粒中的非平衡偏聚 - Determination of critical time of non - equilibrium segregation of tin
锡的非平衡晶界偏聚临界时间确定 - Vacancy - solute atom complexes diffusion and non - equilibrium segregation in alloy steels
溶质原子复合体扩散与非平衡偏聚 - As the aging time increases further , the impact energy is gradually increased and the embrittlement is gradually improved . changing of impact energy with time responses of the kinetics of non - equilibrium segregation , so the time at which the impact energy is minimum is measured as the critical time . as measure in this experiment the critical time of sn non - equilibrium segregation is 120 seconds at 750
冲击功随保温时间的变化反映了sn的非平衡品界偏聚动力学过程,因此把冲击功达到最小值时的保温时’间作为s , 1发生非平衡晶界偏聚的临界时间,本试验测出sn在0 , 15wt . % c钢中750保温时发生非平衡晶界偏聚的临界时间为1205左右。 - This segregation behavior of sn accords with the mechanism of non - equilibrium segregation . it can be obtained through the theoretical calculations that the critical time of sn non - equilibrium segregation is 124 seconds at 750 and the critical cooling rate is 8 / s when cooling from 1320 . it is suggested that controlling the cooling rate during continuous casting to avoid the critical cooling rate ( 8 / s ) and avoiding high stress near the trough temperature ( 750 ) may control the form
通过研究残留元素sn的偏聚机制及其对o . 15wt . % c钢热塑性的影响,对试验钢进行脆性预测:建议在该钢的连铸过程中弯道矫直温度尽量避开塑性谷底温度750 ,二冷区的冷速尽量避开临界冷却速率8 / s ,从而可以减少该低碳钢连铸坯表面裂纹和横向裂纹,提高其成材率。